Bluerox 67-W50 (50% emulsion in water and methanol) for (co)polymerization of vinyl chloride andvinylidine chloride.● 10hr. Half Life Temp: 38 ℃● 1hr. Half Life Temp: 56 ℃● 0.1hr. Half Life Temp: 75 ℃
Bluerox 65-W50 (50% emulsion in water and methanol) for (co)polymerization of vinyl chloride andvinylidine chloride.● 10hr. Half Life Temp: 46 ℃● 1hr. Half Life Temp: 64 ℃● 0.1hr. Half Life Temp: 84 ℃
Bluerox 100-W50 (50% emulsion in water and methanol) for (co) polymerization of vinyl chloride andvinylidine chloride.● 10hr. Half Life Temp: 47 ℃● 1hr. Half Life Temp: 64 ℃● 0.1hr. Half Life Temp: 83 ℃
Bluerox 59-W40 is an initiator (40% water-based emulsion) for (co) polymerization of vinyl chloride and vinylidene chloride. Extremely active initiator developed for the low-temperature polymerization of vinyl chloride to produce high K-value PVC.● 10hr. Half Life Temp: 23 ℃● 1hr. Half Life Temp: 39...
Bluerox 64-C75 is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes● 10hr. Half Life Temp: 57 ℃● 1hr. Half Life Temp: 75 ℃● 0.1hr. Half Life Temp: 94 ℃
Bluerox 67-C75 is an efficient initiator for the production of Low Density Polyethylene (LDPE). It is used both for tubular and autoclave processes.● 10hr. Half Life Temp: 38 ℃● 1hr. Half Life Temp: 56 ℃● 0.1hr. Half Life Temp: 75 ℃
Bluerox 89-E50 is an initiator (40% active ingredient in mineral oil) for (co) polymerization of styrene, acrylonitrile acrylates and methacrylates.● 10hr. Half Life Temp: 94 ℃● 1hr. Half Life Temp: 113 ℃● 0.1hr. Half Life Temp: 134 ℃