Bluerox 89-E50 is an initiator (40% active ingredient in mineral oil) for (co) polymerization of styrene, acrylonitrile acrylates and methacrylates.
● 10hr. Half Life Temp: 94 ℃
● 1hr. Half Life Temp: 113 ℃
● 0.1hr. Half Life Temp: 134 ℃
Product Technical Specifications
| Appearance | Assay | Total active oxygen | Density, -10°C | SADT | Storage temperature Ts max |
|---|---|---|---|---|---|
| Clear colorless liquid | 49.0-51.0% | 6.02-6.27% | 0.962 g/cm³ | 70℃ | 25℃ |
Process & Logistics & Packaging


Polymerization of styrene: Bluerox 89-E50 can be used for the bulk polymerization of styrene in the temperature range between 90 and 120°C. Other applications: Bluerox 89-E50 can also be used for the (co)polymerization of styrene,acrylonitrile, acrylates and methacrylates in the temperature range between 95°C and 125°C.

Class 5.2 type F