Bluerox 87S can be used to crosslink elastomers at intermediate temperatures, a typical crosslink temperature is 150°C. Bluerox 87S is recommended for highly demanding applications e.g. as crosslinker for the polyolefin elastomer copolymer (POE) film in photovoltaic devices.
● 10hr. Half Life Temp: 95 ℃
● 1hr. Half Life Temp: 113 ℃
● 0.1hr. Half Life Temp: 134 ℃
Product Technical Specifications
| Appearance | Assay | Total active oxygen | Inorganic + organic hydrolyzable chloride | SADT | Storage temperature Ts max |
|---|---|---|---|---|---|
| Clear colorless liquid | ≥96.5% | ≥5.93% | ≤50ppm | 55℃ | 20℃ |
Process & Logistics & Packaging


Bluerox 87S can be used to crosslink elastomers at intermediate temperatures, a typical crosslink temperature is 150°C. Bluerox 87S is recommended for highly demanding applications e.g. as crosslinker for the polyolefin elastomer copolymer (POE) film in photovoltaic devices.Bluerox 87 S is used as an initiator for the polymerization or copolymerization of styrene in the temperature range of 100°C to 130°C. In the bulk polymerization process, the advantage of Bluerox 87 S as an initiator is that it can increase the polymerization speed. In the suspension polymerization process: Bluerox 87 S can effectively reduce the residual styrene content in the final product.

Class 5.2 type D